REAEARCH PAPER |
|
|
|
|
|
Influence of Si-O-C Interlayer on the Properties of C/Si-C-N Composites |
LU Guofeng
|
College of Chemistry and Materials, Weinan Normal University, Weinan 714099 |
|
|
Abstract The carbon fiber reinforced Si-C-N ceramic matrix composite with a Si-O-C interlayer(C/Si-O-C/Si-C-N) was fabricated with the matrix fabricated by CVI and the interphase fabricated by PIP. The influence of Si-O-C interlayer on the mechanical properties, oxidation resistance and thermal expansion properties of the composites was investigated. The results indicate that compared to the C/Si-C-N with a pro-carbon interlayer(C/PyC/Si-C-N), the oxidation resistance of C/Si-C-N composite with a Si-O-C interlayer (C/Si-O-C/Si-C-N) was improved. The strength of C/Si-O-C/Si-C-N can compare with that of C/PyC/Si-C-N. The ave-rage coefficient of thermal expansion of C/Si-O-C/Si-C-N was higher than that of C/PyC/Si-C-N throughout the experimental tempe-rature range.
|
Published: 25 August 2017
Online: 2018-05-07
|
|
|
|
1 Lu G F, Qiao S R, Zhang C Y, et al. Oxidation behaviors of carbon fiber reinforced Si-C-N matrix composite[J]. J Chin Ceram Soc,2008,36(11):66(in Chinese). 卢国锋,乔生儒,张程煜,等. 碳纤维增强Si-C-N陶瓷基复合材料的氧化行为[J]. 硅酸盐学报,2008,36(11):66. 2 Labruquère S, Blanchard H, Pailler R, et al. Enhancement of the oxidation resistance of interfacial area in C/C composites.Part Ⅱ: Oxidation resistance of B-C, Si-B-C and Si-C coated carbon preforms densified with carbon[J]. J Eur Ceram Soc,2002,22:1011. 3 Lu G F, et al. Oxidation protection of C/Si-C-N composite by a mullite interphase[J]. Composites Part A,2008,39(9):1467. 4 Lu G F, et al. Oxidation behaviors and mechanisms of C/Si-C-N with a mullite interlayer[J]. Adv Compos Mater,2011,20(2):179. 5 Lu G F, Qiao S R, et al. Structure and flexural behavior of C/mullite/Si-C-N composite[J]. J Mater Eng,2011(9):82(in Chinese). 卢国锋,乔生儒,等. C/Mullite/Si-C-N复合材料的组织结构及其弯曲行为研究[J]. 材料工程,2011(9):82. 6 Saha A, Raj R. Crystallization maps for SiCO amorphous ceramics[J]. J Am Ceram Soc,2007,90(2):578. 7 Kolárˇ F, Machovicˇ V, Svítilová J, et al. Structural characterization and thermal oxidation resistance of silicon oxycarbides produced by polysiloxane pyrolysis[J]. Mater Chem Phys,2004,86:88. 8 Moysan C, Riedel R, et al. Mechanical characterization of a polysiloxane-derived SiOC glass[J]. J Eur Ceram Soc,2007,27:397. 9 Wang S, Chen Z, Ma Q, et al. Effect of fiber surface state on mechanical properties of Cf/Si-O-C composites [J]. Mater Sci Eng A,2005,407:245. 10 Manocha L M, Manocha S M. Studies on solution-derived ceramic coatings for oxidation protection of carbon-carbon composites[J]. Carbon,1995,33(4):435. 11 Lu Guofeng, et al. Fabrication and oxidation behaviors of C/Si-C-N composites[J]. J Mater Eng,2010(3):13(in Chinese). 卢国锋,等. C/Si-C-N复合材料的制备及其氧化行为研究[J]. 材料工程,2010(3):13. 12 Guo W M, Xiao H N, Yasuda E, et al. Oxidation kinetics and mechanisms of a 2D-C/C composite [J]. Carbon,2006,44:3269. 13 Xu Y D, Cheng L F, Zhang L T, et al. Oxidation behavior and mechanical properties of C/SiC composites with Si-MoSi2 oxidation protection coating[J]. J Mater Sci,1999,34:6009. 14 Pantano C G, Singh A K, Zhang H. Silicon oxycarbide glasses[J]. J Sol-Gel Sci Technol,1999,14:7. 15 Baxter R I, Rawlings R D, Iwashita N, et al. Effect of chemical vapor infiltration on erosion and thermal properties of porous carbon/carbon composite thermal insulation[J]. Carbon,2000,38:441. 16 Fei W D, Wang L D. Thermal expansion behavior and thermal mismatch stress of aluminum matrix composite reinforced by β-eucryptite particle and aluminum borate whisker[J]. Mater Chem Phys,2004,85:450. |
|
|
|